Material Notes:
Homopolymer and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewares and toys.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D2240
Tensile Strength, Ultimate 8.00 MPa
1160 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Modulus of Elasticity 0.310 GPa
45.0 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525