Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer

Category Polymer , Thermoplastic , Cyclo Olefin Polymer
Manufacturer Hybrid Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low weight is desired. Hybrid Plastics offers POSS-modified COC plastics that are tough, weather resistant and easily processed. These materials do not use fillers. They exhibit some of the highest heat distortion temperatures at the lowest densities available on the market today. Other modifications are available, so please inquire if there is need for a low density, high temperature material for the application.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Mechanical Properties Metric English Comments
Elongation at Break 13 %
13 %
Flexural Modulus 1.70 GPa

@Temperature 130 °C
247 ksi

@Temperature 266 °F
2.40 GPa

@Temperature 40.0 °C
348 ksi

@Temperature 104 °F
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 155 °C
311 °F
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Processing Properties Metric English Comments
Rear Barrel Temperature 240 - 270 °C
464 - 518 °F
Middle Barrel Temperature 250 - 300 °C
482 - 572 °F
Front Barrel Temperature 260 - 310 °C
500 - 590 °F
Nozzle Temperature 250 - 310 °C
482 - 590 °F
Mold Temperature 90.0 - 115 °C
194 - 239 °F
Descriptive Properties Value Comments