Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Propionate, Molded
Manufacturer Hybrid Plastics
Trade Name Nanoreinforced®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nanoreinforced® Cellulose Propionate Acetate is an optically clear nanocomposite with POSS® dispersed at the nanometer level. Compared to virgin cellulose propionate acetate, it enhances mechanical properties and high use temperatures while maintaining the clarity of cellulose propionate acetate. Other property improvements include fire retardancy, water/oxygen permeation, and oil-chemical resistance.Information provided by Hybrid Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.00 MPa

@Temperature 120 °C
1160 psi

@Temperature 248 °F
23.0 MPa

@Temperature 23.0 °C
3340 psi

@Temperature 73.4 °F
Elongation at Yield 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
160 %

@Temperature 120 °C
160 %

@Temperature 248 °F
Tensile Modulus 1.05 GPa

@Temperature 23.0 °C
152 ksi

@Temperature 73.4 °F
1.40 GPa

@Temperature 120 °C
203 ksi

@Temperature 248 °F
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 94.0 °C
201 °F
Optical Properties Metric English Comments
Refractive Index 1.4711

@Wavelength 644 nm
1.4711

@Wavelength 644 nm
Transmission, Visible 71 - 81 %
71 - 81 %
Copyright © lookpolymers.com All Rights Reserved