Material Notes:
Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength 46.02 MPa
6674 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Strength 63.6 MPa
9230 psi
ASTM D790
Flexural Modulus 2.154 GPa
312.4 ksi
ASTM D790
Izod Impact, Notched 2.94 J/cm
5.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 85.0 °C
185 °F
ASTM D648