IDI Composites A-207 Thermoset Polyester, Sheet

Category Polymer , Thermoset , Composite SMC , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer IDI Composites
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites A-207 Thermoset Polyester, Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion resistance. Excellent paintability.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Water Absorption 0.13 %
0.13 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
ASTM D2583
Tensile Strength, Ultimate 117 MPa
17000 psi
ASTM D638
Flexural Strength 234 MPa
33900 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 221 MPa
32100 psi
ASTM D695
Izod Impact, Notched 13.3 J/cm
24.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 14.2 kV/mm
361 kV/in
ASTM D149