IRPC Polimaxx Polene 1100PK Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1100PK Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: HIGH FLOW, GOOD STIFFNESS, GOOD PROCESSABILITY, GOOD MELT STABILITYAPPLICATIONS: MULTI - FILAMENT FOR BELTS, FIBRES FOR CARPETS INJECTION MOLDING FOR THIN WALL PARTS, HOUSEWARES
Physical Properties Metric English Comments
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 26 %
26 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.250 J/cm²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 200 - 240 °C
392 - 464 °F