Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 37 %
37 %
ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 75.0 °C
167 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 200 - 240 °C
392 - 464 °F
Users viewing this material also viewed the following: