IRPC Polimaxx Porene GA400 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer IRPC Polimaxx
Trade Name Porene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Porene GA400 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:injection moldingelectrical applianceselectrical fansair conditionersfloppy disks
Physical Properties Metric English Comments
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 220 °C
45 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112

@Thickness 6.35 mm,
Temperature 23.0 °C
112

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 41.2 MPa

@Temperature 23.0 °C
5970 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 60.8 MPa

@Temperature 23.0 °C
8820 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.21 GPa

@Temperature 23.0 °C
320 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 1.67 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.12 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 6.35 mm
201 °F

@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C

@Thickness 6.35 mm
187 °F

@Thickness 0.250 in
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Processing Properties Metric English Comments
Processing Temperature 180 - 240 °C
356 - 464 °F
Drying Temperature 80.0 - 90.0 °C

@Time 7200 - 18000 sec
176 - 194 °F

@Time 2.00 - 5.00 hour