ITW Devcon 10 minuteâ„¢ Epoxy, Clear

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer ITW Devcon
Trade Name 10 minute™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon 10 minuteâ„¢ Epoxy, Clear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Viscosity 80000 cP
80000 cP
Mixed Viscosity
Mechanical Properties Metric English Comments
Elongation at Break 5.0 %
5.0 %
Adhesive Bond Strength 16.5 MPa
2400 psi
lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
Tensile Impact Strength 21.0 kJ/m²
10.0 ft-lb/in²
Peel Strength 3.51 - 4.38 kN/m
20.0 - 25.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
dry
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
dry
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
Working time
20.0 min
0.333 hour
Fixture time
90.0 min
1.50 hour
Functional cure
Descriptive Properties Value Comments
Mix ratio (Resin:Hardener) 1:1