ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black

Category Polymer , Adhesive , Thermoset , Polyurethane, TS
Manufacturer ITW Devcon
Trade Name Flexane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
Cured; ASTM D2240
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D412
Elongation at Break <= 600 %
<= 600 %
ASTM D412
Tear Strength 70.1 kN/m
400 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 140
140
H-18 wheel (1000 gram load)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 48.9 °C
120 °F
wet
82.2 °C
180 °F
dry
Shrinkage 12 %
12 %
Cured (shrinkage due to solvent loss); ASTM D2566
Electrical Properties Metric English Comments
Dielectric Strength 13.8 kV/mm
350 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 960 min
16.0 hour
Functional cure
Pot Life 10.0 min

@Temperature 23.9 °C
10.0 min

@Temperature 75.0 °F
Descriptive Properties Value Comments
Coverage per pound, in² @ 1/4" thickness 94
Mix ratio by weight (Resin:Hardener) 94:6