Material Notes:
An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.Fast tacking, low pressure sprayable adhesive with long bonding range, listed under UL INC.® Component recognition category MAGW2 (Adhesives, Isulation), File Number MH6288(N).The solids weight is approximately 35%. The flash point is less than -20°F/less than -29°C. The color is clear/translucent, the consistency is medium liquid, and the application method is spray. The bond range holds up to 60 minutes. Peel strength is 23 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate.Information provided by 3M Adhesives Division.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Uncured
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.0 MPa
2320 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Modulus of Elasticity 0.100 GPa
14.5 ksi
ASTM D638
Adhesive Bond Strength 12.0 MPa
1740 psi
Lap Shear Cohesive Strength; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Users viewing this material also viewed the following: