ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.986 g/cc
0.0356 lb/in³
Mixed
Viscosity 40000 - 60000 cP
40000 - 60000 cP
B
180000 - 220000 cP
180000 - 220000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.1 - 13.8 MPa
1750 - 2000 psi
Elongation at Break 90 - 110 %
90 - 110 %
Tensile Modulus 0.414 - 0.552 GPa
60.0 - 80.0 ksi
Shear Strength 5.86 - 8.27 MPa
850 - 1200 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 20 - 25 min
20 - 25 min
Descriptive Properties Value Comments
Color Blue
Fixture Time 40-45 minutes
Gap Filling Max 1 in
Mix Ratio 10:1
By volume
Users viewing this material also viewed the following: