Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.983 g/cc
0.0355 lb/in³
Mixed
Viscosity 40000 - 60000 cP
40000 - 60000 cP
A
40000 - 60000 cP
40000 - 60000 cP
B
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.7 - 24.1 MPa
3000 - 3500 psi
Elongation at Break 15 - 25 %
15 - 25 %
Tensile Modulus 0.931 - 1.14 GPa
135 - 165 ksi
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 4.0 - 6.0 min
4.0 - 6.0 min
Descriptive Properties Value Comments
Color Cream
Fixture Time 12-15 minutes
Gap Filling Max 0.125 in
Mix Ratio 1:1
By volume