Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.989 g/cc
0.0357 lb/in³
Mixed
Viscosity 1500 - 1800 cP
1500 - 1800 cP
B
1400 - 2000 cP
1400 - 2000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.6 - 31.0 MPa
4000 - 4500 psi
Elongation at Break 5.0 - 10 %
5.0 - 10 %
Tensile Modulus 1.72 - 1.90 GPa
250 - 275 ksi
Shear Strength 13.8 - 17.2 MPa
2000 - 2500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 30 - 35 min
30 - 35 min
Descriptive Properties Value Comments
Color Black
Fixture Time 60-65 minutes
Mix Ratio 2:1