Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.977 g/cc
0.0353 lb/in³
Mixed
Viscosity 50000 - 80000 cP
50000 - 80000 cP
B
80000 - 100000 cP
80000 - 100000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.62 - 10.3 MPa
1250 - 1500 psi
Elongation at Break 5.0 - 15 %
5.0 - 15 %
Tensile Modulus 0.241 - 0.345 GPa
35.0 - 50.0 ksi
Shear Strength 8.96 - 11.0 MPa
1300 - 1600 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 1.0 - 2.0 min
1.0 - 2.0 min
Descriptive Properties Value Comments
Color Off-white
Fixture Time 3-4 minutes
Gap Filling Max 0.125 in
Mix Ratio 10:1
By volume