Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
Mixed
Viscosity 175000 - 220000 cP
175000 - 220000 cP
A
175000 - 220000 cP
175000 - 220000 cP
B
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 - 20.7 MPa
2500 - 3000 psi
Elongation at Break 150 - 180 %
150 - 180 %
Tensile Modulus 0.621 - 0.758 GPa
90.0 - 110 ksi
Shear Strength 11.0 - 13.8 MPa
1600 - 2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 90 - 105 min
90 - 105 min
Descriptive Properties Value Comments
Color Black
Fixture Time 1100 psi in 4 hours
800 psi in 3 hours
Gap Filling Max 1 in
Mix Ratio 1:1
By volume