Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.971 g/cc
0.0351 lb/in³
Mixed
Viscosity 50000 - 80000 cP
50000 - 80000 cP
B
90000 - 120000 cP
90000 - 120000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.8 - 25.5 MPa
3300 - 3700 psi
Elongation at Break 75 - 100 %
75 - 100 %
Tensile Modulus 0.517 - 0.689 GPa
75.0 - 100 ksi
Shear Strength 1.38 - 16.5 MPa
200 - 2400 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 4.0 - 6.0 min
4.0 - 6.0 min
Descriptive Properties Value Comments
Color Off-white, black
Fixture Time 18-25 minutes
Gap Filling Max 1 in
Mix Ratio 10:1
By volume