ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Viscosity 50000 - 80000 cP
50000 - 80000 cP
B
80000 - 110000 cP
80000 - 110000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.1 - 26.2 MPa
3500 - 3800 psi
Elongation at Break 90 - 110 %
90 - 110 %
Shear Strength 15.2 - 18.6 MPa
2200 - 2700 psi
Processing Properties Metric English Comments
Pot Life 15 - 20 min
15 - 20 min
Descriptive Properties Value Comments
Color Off-white, gray
Fixture Time 40-45 minutes
Mix Ratio 10:1
By volume