Imerys Minsparâ„¢ 250 Feldspar

Category Ceramic , Clay , Feldspar Clay , Oxide , Silicon Oxide
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Minspar™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Minsparâ„¢ 250 Feldspar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Imerys
Physical Properties Metric English Comments
Bulk Density 0.993 g/cc
0.0359 lb/in³
loose
1.19 g/cc
0.0428 lb/in³
packed
Particle Size 10.6 µm
10.6 µm
average
Particle Mesh Size 200 Mesh
200 Mesh
0.06% retained
325 Mesh
325 Mesh
1.5% retained
Specific Surface Area 1.5 m²/g
1.5 m²/g
Component Elements Properties Metric English Comments
Al2O3 18.9 %
18.9 %
CaO 1.4 %
1.4 %
Fe2O3 0.050 %
0.050 %
K2O 4.1 %
4.1 %
Loss on Ignition(%) 0.080 %
0.080 %
Na2O 6.8 %
6.8 %
SiO2 68.2 %
68.2 %