Indium Corp. 99.9% InF3 Indium Trifluoride, Anhydrous

Category Ceramic , Halide
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 99.9% InF3 Indium Trifluoride, Anhydrous.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crystalline Form: ColorlessIsomorphous with: AlCl3, YCl3Coordination Number: 6 Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 4.39 g/cc
4.39 g/cc
Solubility in Water 0.040 %
0.040 %
Molecular Weight 171.82 g/mol
171.82 g/mol
Thermal Properties Metric English Comments
Melting Point 1170 °C
2140 °F
Boiling Point >= 1200 °C
>= 2190 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.00010 - 0.0010 %
0.00010 - 0.0010 %
Cadmium, Cd 0.0050 - 0.010 %
0.0050 - 0.010 %
Copper, Cu 0.00050 - 0.0010 %
0.00050 - 0.0010 %
Indium, In 66.83 %
66.83 %
Iron, Fe 0.0010 - 0.0020 %
0.0010 - 0.0020 %
Lead, Pb 0.020 - 0.030 %
0.020 - 0.030 %
Magnesium, Mg 0.00010 - 0.0010 %
0.00010 - 0.0010 %
Nickel, Ni 0.00010 - 0.00050 %
0.00010 - 0.00050 %
Silicon, Si 0.00010 - 0.0010 %
0.00010 - 0.0010 %
Thallium, Tl 0.010 - 0.030 %
0.010 - 0.030 %
Tin, Sn 0.0050 - 0.010 %
0.0050 - 0.010 %