Indium Corp. Indalloy 167 Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 167 Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.2 g/cc
0.405 lb/in³
Thermal Properties Metric English Comments
Melting Point 315 °C
599 °F
Solidus 315 °C
599 °F
Liquidus 315 °C
599 °F
Component Elements Properties Metric English Comments
Antimony, Sb 1.2 %
1.2 %
Gallium, Ga 0.80 %
0.80 %
Lead, Pb 98 %
98 %