Indium Corp. Indalloy® 178 Au-In Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 178 Au-In Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extremely hard, high temperature alloy. Stiff alloy.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 14.9 g/cc
0.538 lb/in³
Thermal Properties Metric English Comments
Melting Point 451 - 485 °C
844 - 905 °F
Solidus 451 °C
844 °F
Liquidus 485 °C
905 °F
Component Elements Properties Metric English Comments
Gold, Au 82 %
82 %
Indium, In 18 %
18 %