Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pb free solder. Zn causes high drossing; corrosion concerns.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.36 g/cc
0.266 lb/in³
Thermal Properties Metric English Comments
Melting Point 174 - 186 °C
345 - 367 °F
Solidus 174 °C
345 °F
Liquidus 186 °C
367 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 3.5 %
3.5 %
Indium, In 4.5 %
4.5 %
Tin, Sn 86.5 %
86.5 %
Zinc, Zn 5.5 %
5.5 %