Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 10.36 g/cc
0.3743 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.4 MPa
5570 psi
Elongation at Break 3.5 %
3.5 %
Thermal Properties Metric English Comments
Specific Heat Capacity 0.150 J/g-°C
0.0359 BTU/lb-°F
Solid
Melting Point 245 - 255 °C
473 - 491 °F
Solidus 245 °C
473 °F
Liquidus 255 °C
491 °F
Component Elements Properties Metric English Comments
Antimony, Sb 10 %
10 %
Lead, Pb 85 %
85 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 ohm-cm
0.0000290 ohm-cm
Users viewing this material also viewed the following: