Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34

Category Metal , Ferrous Metal , Duplex , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion resistance properties. UR 45N with 22% Cr and 3% Mo additions, performs much better than 316L grade in almost all corrosive media,. The yield strength is about twice that of austenitic stainless steels. This allows the designer to save weight and makes the alloy more cost competitive when compared to 316 L grade. Typical operation temperatures are -50°C/+ 280°C (-58°F/+536°F). Lower temperatures uses could to be considered require additional precautions, in particular for welded structures. UR 45N is a multi-purposes material which can be used in various corrosive media. Typical applications are Pulp and Paper industry, Oil and Gas industry, Pollution control equipments, Chemical industry and Chemical tankers.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 210 - 240
210 - 240
Typical
Hardness, Rockwell C 15 - 20
15 - 20
Typical
Tensile Strength, Ultimate >= 680 MPa
>= 98600 psi
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %
>= 66700 psi

@Strain 0.200 %
>= 490 MPa

@Strain 1.00 %
>= 71100 psi

@Strain 1.00 %
Elongation at Break >= 25 %
>= 25 %
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.333
0.333
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Charpy Impact >= 120 J
>= 88.5 ft-lb
150 J
111 ft-lb
Typical
>= 75.0 J

@Temperature -50.0 °C
>= 55.3 ft-lb

@Temperature -58.0 °F
90.0 J

@Temperature -50.0 °C
66.4 ft-lb

@Temperature -58.0 °F
Typical
Thermal Properties Metric English Comments
CTE, linear 13.5 µm/m-°C

@Temperature 20.0 - 100 °C
7.50 µin/in-°F

@Temperature 68.0 - 212 °F
14.0 µm/m-°C

@Temperature 20.0 - 200 °C
7.78 µin/in-°F

@Temperature 68.0 - 392 °F
14.5 µm/m-°C

@Temperature 20.0 - 300 °C
8.06 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 °C
0.108 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 22 %
22 %
Iron, Fe 69.518 - 69.52 %
69.518 - 69.52 %
As remainder
Molybdenum, Mo 3.0 %
3.0 %
Nickel, Ni 5.3 %
5.3 %
Nitrogen, N 0.16 %
0.16 %
Sulfur, S <= 0.0020 %
<= 0.0020 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F