Ineos ABS Lustran® 348

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Ineos ABS
Trade Name Lustran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® 348.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features:UnfilledSuitable processing methods:Injection molding
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Melt Flow 17 g/10 min

@Load 10.0 kg,
Temperature 220 °C
17 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.2 MPa
6990 psi
Elongation at Break 25 %
25 %
Nominal
Elongation at Yield 3.5 %
3.5 %
Tensile Modulus 2.62 GPa
380 ksi
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL Recognized
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Injection Molding
Mold Temperature 60.0 °C
140 °F
Injection Molding
Injection Velocity 200 mm/sec
7.87 in/sec
Injection Pressure 55.0 MPa
7980 psi