Material Notes:
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 black) resin meets or exceeds ASTM D 3965 3-2-2-2-2 cell class requirements for ASTM F 628 and D 2661. It is also listed under NSF Standard 14.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM-D638
Tensile Modulus 2.10 GPa
305 ksi
ASTM-D638
Izod Impact, Notched 1.87 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
3.50 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM-D256
3.74 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.01 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 6.35 mm
212 °F

@Thickness 0.250 in
Annealed; ASTM-D648
Processing Properties Metric English Comments
Melt Temperature 232 - 243 °C
450 - 469 °F
Injection Molding
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Drying Temperature 82.0 - 93.0 °C

@Time 7200 sec
180 - 199 °F

@Time 2.00 hour
Moisture Content <= 0.050 %
<= 0.050 %
Dew Point <= -29.0 °C
<= -20.2 °F
inlet air
Descriptive Properties Value Comments
Injection Pressure Moderately High to High, Injection Molding
Injection Speed Moderate to Fast
Injection Molding