Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos ABS Lustran® LGA-SF  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® LGA-SF  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 220 °C
25 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.5 MPa
5870 psi
Elongation at Break 26 %
26 %
Nominal
Elongation at Yield 3.4 %
3.4 %
Tensile Modulus 2.13 GPa
309 ksi
Charpy Impact, Notched 2.10 J/cm²
9.99 ft-lb/in²
0.650 J/cm²

@Temperature -30.0 °C
3.09 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
Vicat Softening Point 94.0 °C
201 °F
50°C/h 50N
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Injection Molding
Mold Temperature 60.0 °C
140 °F
Injection Molding
Injection Velocity 200 mm/sec
7.87 in/sec
Injection Pressure 55.0 MPa
7980 psi
Users viewing this material also viewed the following: