Material Notes:
Lustran® SAN DN77 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for use in compounding.
Physical Properties Metric English Comments
Melt Flow 14 g/10 min

@Load 3.80 kg,
Temperature 230 °C
14 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM-D638
Flexural Strength 75.8 MPa
11000 psi
at Fail; ASTM-D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM-D790
Izod Impact, Unnotched 3.20 J/cm
6.00 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Vicat Softening Point 109 °C

@Load 1.00 kg
228 °F

@Load 2.20 lb
120°C/hour; ASTM-D1525
Descriptive Properties Value Comments
Acrylonitrile Content (%) 32.5
Users viewing this material also viewed the following: