Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos ABS NOVODUR® KU 2-5300 ABS, Injection Grade  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS NOVODUR® KU 2-5300 ABS, Injection Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection molding grade, high heat resistance and toughness, low-emission.Applications: Automotive parts, household goods.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued prior to Styrolution's acquisition of the Novodur product line.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7110 psi
Elongation at Yield 2.7 %
2.7 %
Tensile Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched NB
NB
0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 3.20 J/cm²
15.2 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Vicat Softening Point 106 °C
223 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Users viewing this material also viewed the following: