Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H00G-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H00G-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A polypropylene homopolymer produced by Ineos utilizing catalyst technology. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. Homopolymer H00G-00 meets certain automotive resin specifications.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ASTM D2240
Tensile Strength, Ultimate 20.7 MPa
3000 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 35.8 MPa
5190 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 100 %
100 %
2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 10 %
10 %
2 in/min.; ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
Secant @ 1% strain; ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched >= 13.35 J/cm
>= 25.01 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Blow Molding
Extrusion
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved