Material Notes:
This is a controlled rheology general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of film and profile extrusion applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer ProductsIndustrial ProductsBOPP FilmExtrusionBenefitsEase of processingHigh throughputGood balance of propertiesInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.3 MPa

@Temperature 23.0 °C
4970 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 12.7 %
12.7 %
ASTM D638
Flexural Modulus, 1% Secant 1430 MPa

@Temperature 23.0 °C
207000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Izod Impact, Notched 0.481 J/cm

@Temperature 23.0 °C
0.900 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved