Material Notes:
A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release properties. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ASTM D2240
Tensile Strength at Break 24.1 MPa
3500 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 38.6 MPa
5600 psi
2 in/min.; ASTM D638
Elongation at Break 16 %
16 %
2 in/min.; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2 in/min.; ASTM D638
Flexural Modulus 1.793 GPa
260.1 ksi
Secant @ 1% strain; ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Injection
Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution