Ineos N01N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos N01N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properties, and combines high heat resistance with good gloss and thermoformability. This grade meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:Food service trays, containersRigid packagingBenefits:Very broad temperature performance rangeHigh stiffnessLow temperature impactThermoformability
Physical Properties Metric English Comments
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break >= 25 %
>= 25 %
ASTM D638
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790B
Izod Impact, Notched 0.374 J/cm

@Temperature -20.0 °C
0.700 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
245 °F
ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution