Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos N20N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos N20N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high melt flow rate, nucleated polypropylene impact copolymer formulated for improved flowability. It has an optimum balance of stiffness and impact resistance for injection molded applications. This grade is vis broken and has antistat and a slip agent. It is particularly well suited for the Materials Handling industry in applications such as crates for food transport and storage. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsMaterials handling products (crates)Consumer products (pails, small containers)Industrial applicationsBenefitsMedium to High impact resistanceGood impact to stiffness balanceSuperior moldabilityInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 61
61
ASTM D785
Tensile Strength, Yield 20.7 MPa

@Temperature 23.0 °C
3000 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 5.9 %
5.9 %
ASTM D638
Flexural Modulus, 1% Secant 965 MPa

@Temperature 23.0 °C
140000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Izod Impact, Notched 1.39 J/cm

@Temperature -20.0 °C
2.60 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Descriptive Properties Value Comments
Instrumented Impact (Dynatup) Ductile
23°C, D3763
Ductile
negative 20°C, D3763
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: