Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos Nova 4210 Medium Impact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova 4210 Medium Impact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 3.5 g/10 min
3.5 g/10 min
Condition G
Mechanical Properties Metric English Comments
Hardness, Rockwell M 57
57
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Modulus of Elasticity 2.759 GPa
400.2 ksi
ASTM D638
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.759 GPa
400.2 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm

@Diameter 3.17 mm
0.993 ft-lb/in

@Diameter 0.125 in
bar, 0.010" notch radius; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C

@Temperature 20.0 °C
41.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 2.59

@Frequency 1e+6 Hz
2.59

@Frequency 1e+6 Hz
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Melt Temperature 190 - 274 °C
374 - 525 °F
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved