Ineos Nova S-5100 High Impact Compact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova S-5100 High Impact Compact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
DIN 53479
Water Absorption <= 0.10 %
<= 0.10 %
DIN 53495
Melt Flow 2.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
DIN 5375/ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
DIN 53455
Elongation at Break 10 %
10 %
DIN 53455
Modulus of Elasticity 2.55 GPa
370 ksi
DIN 53457
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
DIN 53453/ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Vicat Softening Point 99.0 °C
210 °F