Material Notes:
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used after expansion for cellular bricks.Applications: This grade is mainly used for cellular bricks application.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density >= 0.0120 g/cc
>= 0.000434 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
0.420 - 0.820 mm
0.0165 - 0.0323 in
> 95% in this range per Berre Laboratory Analytical Methods 0492
Chemical Properties Metric English Comments
Styrene Content <= 0.10 %
<= 0.10 %
Residual Styrene Monomer Content per Berre Laboratory Analytical Methods 0075
Blowing Agent Content >= 5.8 %
>= 5.8 %