Ineos R08S-00 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos R08S-00 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a medium flow rate random copolymer designed for extrusion processing requiring slip properties and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsCast FilmExpanded PP BeadsBlow moldingInjection moldingThermoformingBenefitsSuperior slip propertiesConsistent processingInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Yield 13.6 %
13.6 %
ASTM D638
Flexural Modulus, 1% Secant 724 MPa
105000 psi
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.4 °C
157 °F
ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution