Ineos R55C-00 Clarified Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos R55C-00 Clarified Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling capabilities, excellent clarity, fast cycle times and good stiffness-to-impact properties balance. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520. Preliminary properties listed below could later be subject to minor change.Applications:Thin wall injection molding (TWIM) of multi-cavity partsStadium cups and containersAudio/video media rigid packaging formatsConsumer products and housewaresBenefits:High flow rate for easier mold fillingHigh clarity in thin-walled partsFast cyclingLow bloom and good static charge dissipationVery good impact resistanceInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 230 °C
55 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 84.4
84.4
ASTM D785
Tensile Strength, Yield 29.3 MPa
4250 psi
ASTM D638
Flexural Modulus 1.073 GPa
155.6 ksi
ASTM D790A
Izod Impact, Notched 0.486 J/cm
0.910 ft-lb/in
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.7 °C
184 °F
ASTM D648
Optical Properties Metric English Comments
Haze 17.3 %
17.3 %
50-mil plaque, % Diffuse Transmittance; ASTM D1003
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution