High-impact grade of polystyrene with excellent ESCR.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
50% RH
Water Absorption at Saturation <= 0.10 %
<= 0.10 %
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 2.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 45
45
ASTM D785
Tensile Strength, Ultimate 26.0 MPa
3770 psi
ASTM D638
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 65 %
65 %
ASTM D638
Tensile Modulus 1.10 GPa
160 ksi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790-1
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Gardner Impact 17.0 J

@Thickness 3.17 mm
12.5 ft-lb

@Thickness 0.125 in
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 101 °C
214 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Gloss 15 %
15 %
60°; ASTM D523
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F