Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive components.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 0.890 g/cc

@Temperature 23.0 °C
0.0322 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 9.0 %
9.0 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 0.800 GPa
116 ksi
1 mm/min; ISO 527-1,-2
Flexural Modulus 0.900 GPa
131 ksi
2 mm/min; ISO 178
Charpy Impact, Notched 0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-1,-2
Descriptive Properties Value Comments
Color Black