Material Notes:
INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automotive components.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 0.910 g/cc

@Temperature 23.0 °C
0.0329 lb/in³

@Temperature 73.4 °F
ISO 1183
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ISO 294
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 294
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 0.50 %

@Temperature 900 °C
0.50 %

@Temperature 1650 °F
ISO 3451-1/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 7.5 %
7.5 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 1.00 GPa
145 ksi
1 mm/min; ISO 527-1,-2
Charpy Impact, Notched 0.650 J/cm²

@Temperature -30.0 °C
3.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ISO 75-1,-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
FMVSS 302
Descriptive Properties Value Comments
Automotive Materials Pass
FMVSS 302
Color Natural
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved