Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 4-8000 is a polypropylene random copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 4-8000 is highly suitable for pressure pipe manufacturing, including hot, drinking water systems and floor-heating application.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 0.900 g/cc

@Temperature 23.0 °C
0.0325 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 13 %
13 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 0.900 GPa
131 ksi
1 mm/min; ISO 527-1,-2
Charpy Impact Unnotched 3.00 J/cm²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ISO 75-1,-2
Descriptive Properties Value Comments
Color Natural