Intercontinental Polymers 728-01 PET Polymer Type - Clear, Polyester Pellets

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Intercontinental Polymers, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers 728-01 PET Polymer Type - Clear, Polyester Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Filament YarnInformation provided by Intercontinental Polymers.
Physical Properties Metric English Comments
Viscosity Measurement 0.635 - 0.665
0.635 - 0.665
Intrinsic; LCL-PR21
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Gardner Color Number 4.4 - 6.6
4.4 - 6.6
+ b; LCL-PR01
70 - 80
70 - 80
Rd; LCL-PR01
Processing Properties Metric English Comments
Melt Temperature 255 °C
491 °F
LCL-PR29
Moisture Content <= 0.25 %
<= 0.25 %
LCL-PR08
Descriptive Properties Value Comments
COOH 25 - 55 meq/kg
LCL-PR09
DEG 0.6 - 1 wt%
LCL-PR11