Iran Petrochemical (PCC) EP2C 37 F Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EP2C 37 F Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EP2S 37 F offers good process ability, excellent clarity and gloss and exhibits very good heat weld ability.Applications: packaging of stationery, packaging of food stuffs, lamination.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min
6.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868
Tensile Stress 25.0 MPa
3630 psi
ISO R527
Elongation at Yield 14 %
14 %
ISO R527
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 135 °C
275 °F
ISO 306/A
Heat Distortion Temperature 82.0 °C
180 °F
ISO 75/B
Optical Properties Metric English Comments
Haze 1.8 %
1.8 %
MTM 17031
Gloss 85 %
85 %
MTM 17021