Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
I2 (HB 7250) is a high density polyethylene with Propylene as comonomer. It is easy flowing, low warpage, less hard and stiff than I1.Applications: household articles, closures/seals, packaging.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Environmental Stress Crack Resistance 1.0 hour

@Pressure 2.50 MPa
1.0 hour

@Pressure 363 psi
ISO CD 16770
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
28 g/10 min

@Load 5.00 kg,
Temperature 190 °C
28 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break >= 1000 %
>= 1000 %
ISO 527
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 64.0 °C
147 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 136 °C
277 °F
200 - 280 °C
392 - 536 °F