Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) MF3313 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded , High Density Polyethylene (HDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) MF3313 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.933 g/cc
0.0337 lb/in³
ISO 1183
Melt Flow 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
12.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ISO 527-1
Film Elongation at Break, TD 600 %
600 %
ISO 527-1
Tensile Modulus 0.620 GPa
89.9 ksi
ISO 527-1
Elmendorf Tear Strength MD 33.6 g
33.6 g
ISO 6383-2
Elmendorf Tear Strength TD 204 g
204 g
ISO 6383-2
Film Tensile Strength at Break, MD <= 55.0 MPa
<= 7980 psi
ISO 527-1.3
Film Tensile Strength at Break, TD <= 43.0 MPa
<= 6240 psi
ISO 527-1.3
Thermal Properties Metric English Comments
Vicat Softening Point 116 °C
241 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 124 °C
255 °F
Users viewing this material also viewed the following: