Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade S-7054 has high porosity. Therefore it is most suitable for flexible applications. The electrical, mechanical & thermal properties expected of the various applications can be achieved with this grade.Applications: extrusion of flexible sections and hoses, cable industryInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Bulk Density 0.490 g/cc
0.0177 lb/in³
DIN-53466
Volatiles <= 0.20 %
<= 0.20 %
weight %; ISO R-1269
Viscosity Test 105 cm³/g
105 cm³/g
DIN-53726
Ash <= 0.050 %
<= 0.050 %
Sulfate ash, weight %; DIN-53568/2
Component Elements Properties Metric English Comments
Chlorine, Cl 56 %
56 %
by weight
Descriptive Properties Value Comments
Dark Resin, particles 30
per 250 g PVC; HULS-6.9
K-Value 70
DIN-53726
Residual Vinyl Chloride Monomer, ppm =1
HULS-6.11