Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PSU Polysulfone

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PSU Polysulfone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrical insulating productsRigidHigh chemical, fire and temperature resistanceInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
DIN 53479
Water Absorption 0.30 %
0.30 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 69
69
ASTM D785
Tensile Strength 70.0 MPa
10200 psi
DIN 53455
Elongation at Break 50 %
50 %
DIN 53455
Tensile Modulus 2.70 GPa
392 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 56.0 µm/m-°C
31.1 µin/in-°F
DIN 52328
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 190 °C
374 °F
DIN 53736
Maximum Service Temperature, Air 150 °C
302 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 25.0 - 30.0 kV/mm
635 - 762 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Amber/Yellow Translucent
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved